YBG-10 | 6 | 600 | 4.5 | 360 | 10 | 800 | 8.2-10 | 65-80 | -0.03 | -0.2 | 120 |
YBG-12 | 7 | 700 | 5 | 400 | 10 | 800 | 10-12 | 80-95 | -0.03 | -0.2 | 120 |
PLASTIC BONDED SMCO |
BSMCO-3 | 3.0-4.0 | 300-400 | 2.5-3.5 | 199-279 | 9.0-15.0 | 716-1194 | 2.5-3.5 | 20-28 | -0.04 | -0.2 | 120 |
BSMCO-5 | 3.5-5.5 | 350-550 | 3.1-4.5 | 247-358 | 9.0-15.0 | 716-1194 | 4.0-6.5 | 32-52 | -0.04 | -0.2 | 120 |
BSMCO-8 | 5.5-6.8 | 550-680 | 4.2-5.8 | 334-462 | 9.0-15.0 | 716-1194 | 6.0-8.0 | 48-64 | -0.04 | -0.2 | 120 |
1. The above-mentioned data of magnetic parameters and physical properties are given at room temperature.
2. The above values also have relationship to products’ shapes and dimensions. It is recommended that the final Test date be fixed on actual products.
1. Very expensive and brittle, offers high operating temperatures up to 350°C, remarkable resistance against corrosion.
2.SmCo1:5 magnet is also named SmCo5.Prorated with metallic samarium, cobalt and metallic praseodymium , are firstly those roughcasts with different properties and grades after series technology processing from melting, milling, and pressing to sintering in order
3.The (BH) max range is from 16 to 25, maximum working temperature 250°C.
4.The physical character and ductibility of SmCo5 is better than Sm2Co17, so SmCo5 is slightly easier to be machined thin thickness disc or ring wall and complex shapes while Sm2Co17 is more brittle.